Characterization of Polydopamine Thin Films Deposited at Short Times by Autoxidation of Dopamine
Citations Over TimeTop 1% of 2013 papers
Abstract
Current interest in melanin films derived from the autoxidation of dopamine stems from their use as a universal adhesion layer. Here we report chemical and physical characterization of polydopamine films deposited on gold surfaces from stirred basic solutions at times ranging from 2 to 60 min, with a focus on times ≤10 min. Data from Fourier transform infrared (FTIR), X-ray photoelectron spectroscopy (XPS), and electrochemical methods suggest the presence of starting (dopamine) and intermediate (C=N-containing tautomers of quinone and indole) species in the polydopamine films at all deposition times. A uniform overlayer analysis of the XPS data indicates that film thickness increased linearly at short deposition times of ≤10 min. At deposition times ≥10 min, the films appeared largely continuous with surface roughness ≈ ≤ 2 nm, as determined by atomic force microscopy (AFM). Pinhole-free films, as determined by anionic redox probe measurements, required deposition times of 60 min or greater.
Related Papers
- → Autoxidation of ketones and esters in basic solution(1971)30 cited
- → The autoxidation of aliphatic esters. Part 2. The autoxidation of neopentyl esters(2000)15 cited
- → Analysis of High Molecular Weight Autoxidation Products Using High Performance Size Exclusion Chromatography: I. Changes During Autoxidation(1993)13 cited
- → Autoxidation of Unsaturated Fatty Acid Methyl Esters. I.(1978)5 cited
- → Tocopherols as Antioxidants in Autoxidation of Methyl. Linoleate. II.(1977)