Self-assembled zinc(ii) Schiff base polymers for applications in polymer light-emitting devices
Chemical Communications2004Iss. 23, pp. 2758–2758
Citations Over TimeTop 11% of 2004 papers
Abstract
Thermally stable zinc(II) Schiff base polymers (decomposition temperature up to 461 degrees C; M(n)= 13580 to 20440) formed by self-assembly reactions of zinc(II) salts and salicylaldimine monomers exhibit blue to yellow PL with quantum yields up to 0.34 in DMF; PLEDs employing these polymers as emitters give green or orange EL with turn-on voltage at 5 and 6 V and maximum efficiency of 2.0 and 2.6 cd A(-1) respectively.
Related Papers
- → Zinc gluconate and zinc sulphate as dietary zinc sources for Atlantic salmon(2001)48 cited
- → Effects of Dietary Zinc upon Tissue Zinc and Percent Unsaturated Plasma-Zinc Binding Capacity(1979)22 cited
- → Contribution of zinc fraction to available zinc extracted, by some chemical methods, from rice growing soils of North-Western Himalayas(1990)6 cited
- → Effect of time of application on the effectiveness of zinc sulphate and zinc oxide as sources of zinc for wheat(1988)3 cited
- → Local absorption of zinc from wounds treated with different concentrations of zinc sulphate(1978)4 cited