Control of pyrite surface chemistry in physical coal cleaning
Abstract
To better understand the flotation behavior of coal pyrite, studies have been initiated to characterize the floatability of coal pyrite and mineral pyrite. The hydrophobicity of coal material pyrite was examined over a range of pH and oxidation times. The results indicate that surface oxidation plays an important role in coal and mineral pyrite hydrophobicity. The hydrophobicity of mineral pyrite decreases with increasing oxidation time (20 min. to 5 hr.) and increasing pH (pH 4.6 to 9.2), with maximum depression occurring at pH 9.2. However, coal pyrite exhibited low floatability, even at the lowest oxidation time, over the entire pH range. X-ray photoelectron spectroscopy (XPS) results suggest the growth of an oxidized iron layer as being responsible for the deterioration in floatability, while a sulfur-containing species present on the sample surfaces may promote floatability. Preliminary studies of the effect of frother indicate an enhancement in the floatability of both coal and mineral pyrite over the entire pH range.
Related Papers
- → Genesis and Distribution of Pyrite in the Lacustrine Shale: Evidence from the Es3x Shale of the Eocene Shahejie Formation, Zhanhua Sag, East China(2021)33 cited
- → Intermediary sulfur compounds in pyrite oxidation: implications for bioleaching and biodepyritization of coal(1999)104 cited
- → As(V) and As(III) reactions on pristine pyrite and on surface-oxidized pyrite(2012)51 cited
- → Controlling incipient oxidation of pyrite for improved rejection. Eighth quarterly technical progress report, July 1, 1994--September 30, 1994(1994)
- Experimental study on secondary processing of sulfur concentrate containing arsenic(2011)