Atomic Layer Deposition of Platinum Thin Films
Chemistry of Materials2003Vol. 15(9), pp. 1924–1928
Citations Over TimeTop 10% of 2003 papers
Abstract
Platinum thin films were grown at 300 °C by atomic layer deposition (ALD) using (methylcyclopentadienyl)trimethylplatinum (MeCpPtMe3) and oxygen as precursors. The films had excellent uniformity, low resistivity, and low-impurity contents. Structural studies by X-ray diffraction showed that the films were strongly (111) oriented. Growth rates of 0.45 Å cycle-1 were obtained with 4 s total cycle times. The film thickness was found to linearly depend on the number of the reaction cycles. Also, the possible reaction mechanism is discussed.
Related Papers
- → Spatial atomic layer deposition: A route towards further industrialization of atomic layer deposition(2011)373 cited
- → Characteristics and applications of plasma enhanced-atomic layer deposition(2011)103 cited
- → ALD: Atomic Layer Deposition – Precise and Conformal Coating for Better Performance(2014)14 cited
- → A Study of Surface Oxides on Platinum Electrodes(1964)48 cited
- → Application of atomic layer deposition in nanophotonics(2014)2 cited